COBALT
Quote, Buy, Track!
We make it easy to get instant pricing and purchase your metal at the click of a button. Track your order progress, get notified when it ships, and follow your shipment online until it’s delivered. It’s that easy!
Latest Articles
Best Practices When Using Specialty Materials for SWRO Feed and Brine Reject Lines
In our webinar we 8217 ll explore the fascinating journey of stainless steels in SWRO Seawater Reverse Osmosis applications <
2024 Trade Shows
Come talk to a Rolled Alloys representative in person about your project You can find us at these trade shows
Los Angeles Operations Tour
Welcome to Rolled Alloys Los Angeles where our General Manager Carol Plana with nearly two decades of experience leads an
Dual Certification
The term 8220 dual certification 8221 is primarily employed when certifying a material as meeting the specifications for two separate
René 41
René 41 is an age hardening nickel base superalloy with exceptional strength from room temperature through about 1600°F. The alloy is sensitive to strain age cracking during welding. Sound welds can be made by the resistance and electron beam methods. GTAW using DC straight polarity requires good joint fit-up and cooling by means of copper backup bars or water-cooled fixtures. René 41 should be in the fully solution treated condition prior to welding. After welding the assembly should be solution treated using rapid heating and cooling rates through the 1200-1600°F range, followed by aging.
Mechanical properties vary with the solution and aging treatments. Higher solution temperatures result in better room temperature ductility and elevated temperature creep-rupture strength. Lower solution temperatures give higher tensile strengths. Two commonly used heat treatments are:
1. Solution treat: 2150°F 4 hours, air cool. Age: Reheat 1650 °F 4 hours, air cool.
2. Solution treat: 1975 °F 4 hours, air cool. Age: Reheat 1400°F 16 hours, air cool.
- Exceptionally high strength
- Oxidation resistant through 1800°F
UNS: N07041
W. NR.: 2.4973
AMS: 5545, 5712, 5713, 5800
GE: B50TF109, B50T59, B50TF76
- Jet engine hot components
- Missile components
- Bolting
- Springs