STAINLESS STEEL
Quote, Buy, Track!
We make it easy to get instant pricing and purchase your metal at the click of a button. Track your order progress, get notified when it ships, and follow your shipment online until it’s delivered. It’s that easy!
Latest Articles
Best Practices When Using Specialty Materials for SWRO Feed and Brine Reject Lines
In our webinar we 8217 ll explore the fascinating journey of stainless steels in SWRO Seawater Reverse Osmosis applications <
2024 Trade Shows
Come talk to a Rolled Alloys representative in person about your project You can find us at these trade shows
Los Angeles Operations Tour
Welcome to Rolled Alloys Los Angeles where our General Manager Carol Plana with nearly two decades of experience leads an
Dual Certification
The term 8220 dual certification 8221 is primarily employed when certifying a material as meeting the specifications for two separate
440C
Stainless 440C is a high-carbon martensitic stainless steel. As a martensitic stainless steel, 440C is magnetic and can be hardened by heat treatment. The high carbon content in 440C provides high hardness and strength. Despite this carbon content, the chromium content is sufficient to retain its stainless characteristics.
Martensitic steels are commonly used in applications where high strength and moderate corrosion resistance is required.
- Attains the highest hardness of any stainless steel, when heat-treated
- Highest carbon content of 400 series stainless steels
UNS: S44004
W. Nr.: 1.4125
ASTM: A 276
ASME: SA 276
AMS: 5630, 5880
440C Round Bar
- Valve Seats
- Surgical Instruments
- Bearings
- Bushings
- Nozzles
- Structural Aircraft Parts