STAINLESS STEEL
Quote, Buy, Track!
We make it easy to get instant pricing and purchase your metal at the click of a button. Track your order progress, get notified when it ships, and follow your shipment online until it’s delivered. It’s that easy!
Latest Articles
Best Practices When Using Specialty Materials for SWRO Feed and Brine Reject Lines
In our webinar we 8217 ll explore the fascinating journey of stainless steels in SWRO Seawater Reverse Osmosis applications <
2024 Trade Shows
Come talk to a Rolled Alloys representative in person about your project You can find us at these trade shows
Los Angeles Operations Tour
Welcome to Rolled Alloys Los Angeles where our General Manager Carol Plana with nearly two decades of experience leads an
Dual Certification
The term 8220 dual certification 8221 is primarily employed when certifying a material as meeting the specifications for two separate
PRODEC® 303
Rolled Alloys Machining Quality (PRODEC®) 303 is a fully resulfurized free-machining austenitic stainless steel melted and processed to maximize machinability. It should be considered for automatic screw machines where extensive machining is required. PRODEC® 303 is nonmagnetic in the annealed condition but may become slightly magnetic as a result of cold working.
PRODEC® 303 is resistant to mildly corrosive atmospheres but is inferior to 304 because of the high sulfur content. For optimum corrosion resistance, it is recommended that PRODEC® 303 be chemically treated to remove sulfides from the final surface of the parts.
The high sulfur content, added for machinability, is detrimental to hot workability. If hot forming is necessary, PRODEC® 304 or an intermediate sulfur level should be considered. When forging is necessary, it should be done in the 1800-2200°F range, and should be followed by annealing at 1900°F minimum and water quenching or rapid cooling by other means.The cold formability of PRODEC® 303 is limited by the sulfur content. Bending with a generous bend radius may be considered for PRODEC® 303. When cold forming is required, PRODEC® 304 should be considered.
PRODEC® 303 is not recommended for applications requiring welding. The high sulfur level in PRODEC® 303 makes it prone to weld solidification cracking. If welding is necessary, AWS E312 filler metal may be considered.
PRODEC® 303 is easily machined and produces small brittle chips. PRODEC® 303 may be machined at high speeds with deep cuts and heavy feeds on powerful, rigid equipment using good lubricants and sharp tooling.
- Melted and processed to maximize machinability
- Improved machinability over 304/304L and 316/316L
UNS: S30300
W. NR.: 1.4305
ASTM: A 582
AMS: 5640
PRODEC® 303 Hex Bar, PRODEC® 303 Round Bar
- Automatic screw machines