STAINLESS STEEL
Quote, Buy, Track!
We make it easy to get instant pricing and purchase your metal at the click of a button. Track your order progress, get notified when it ships, and follow your shipment online until it’s delivered. It’s that easy!
Latest Articles
Best Practices When Using Specialty Materials for SWRO Feed and Brine Reject Lines
In our webinar we 8217 ll explore the fascinating journey of stainless steels in SWRO Seawater Reverse Osmosis applications <
2024 Trade Shows
Come talk to a Rolled Alloys representative in person about your project You can find us at these trade shows
Los Angeles Operations Tour
Welcome to Rolled Alloys Los Angeles where our General Manager Carol Plana with nearly two decades of experience leads an
Dual Certification
The term 8220 dual certification 8221 is primarily employed when certifying a material as meeting the specifications for two separate
321
321 stainless is a titanium stabilized grade commonly used for service in the 1000-1600°F temperature range. For service temperatures up to about 1600°F, a stabilizing treatment at 1550-1650°F, air cool, may be used to provide optimum resistance to intergranular corrosion and to polythionic acid stress corrosion cracking.
321 stainless is readily welded by all common methods including submerged arc. Appropriate weld fillers are AWS ER347 bare wire and E347 covered electrodes. 321 stainless is similar in machinability to 304 stainless steel. It has a machinability rating of 45% relative to AISI B1112.
- Oxidation resistant to 1600°F
- Stabilized against weld heat affected zone (HAZ) intergranular corrosion
- Resists polythionic acid stress corrosion cracking
UNS: S32100
W. NR.: 1.4541
ASTM: A 240, A 276, A 312, A 479
ASME: SA 240, SA 276, SA 312, SA 479
AMS: 5510, 5645
QQS: 763, 766D
- Aircraft piston engine manifolds
- Expansion joints
- Thermal oxidizers
- Refinery equipment
- High temperature chemical process equipment