STAINLESS STEEL
Quote, Buy, Track!
We make it easy to get instant pricing and purchase your metal at the click of a button. Track your order progress, get notified when it ships, and follow your shipment online until it’s delivered. It’s that easy!
Latest Articles
Best Practices When Using Specialty Materials for SWRO Feed and Brine Reject Lines
In our webinar we 8217 ll explore the fascinating journey of stainless steels in SWRO Seawater Reverse Osmosis applications <
2024 Trade Shows
Come talk to a Rolled Alloys representative in person about your project You can find us at these trade shows
Los Angeles Operations Tour
Welcome to Rolled Alloys Los Angeles where our General Manager Carol Plana with nearly two decades of experience leads an
Dual Certification
The term 8220 dual certification 8221 is primarily employed when certifying a material as meeting the specifications for two separate
410S
Alloy 410S stainless steel is a low carbon modification of Type 410 stainless steel. Low carbon and optionally a small addition of titanium and/ or columbium minimize austenite formation at high temperatures, thereby restricting the alloy’s ability to harden. The material remains soft and ductile even when the material is rapidly cooled from above the critical temperature. This low hardening characteristic helps to prevent cracking when the steel is welded or exposed to high temperatures. The alloy is completely ferritic in the annealed condition. 410S is ferromagnetic.
- Increased weldability over 410
- Maintains ductility even when heated and quenched
UNS: S41008
W. NR.: 1.4000
ASTM: A 240
ASME: SA 240
- Tower packing
- Distillation trays
- Automotive exhaust components
- Quenching racks