NICKEL
Quote, Buy, Track!
We make it easy to get instant pricing and purchase your metal at the click of a button. Track your order progress, get notified when it ships, and follow your shipment online until it’s delivered. It’s that easy!
Latest Articles
Best Practices When Using Specialty Materials for SWRO Feed and Brine Reject Lines
In our webinar we 8217 ll explore the fascinating journey of stainless steels in SWRO Seawater Reverse Osmosis applications <
2024 Trade Shows
Come talk to a Rolled Alloys representative in person about your project You can find us at these trade shows
Los Angeles Operations Tour
Welcome to Rolled Alloys Los Angeles where our General Manager Carol Plana with nearly two decades of experience leads an
Dual Certification
The term 8220 dual certification 8221 is primarily employed when certifying a material as meeting the specifications for two separate
718
- Good mechanical properties: tensile, fatigue and creep-rupture
- Excellent welding characteristics, resistant to postweld age cracking
- Oxidation resistant throughout its useful temperature range
UNS: N07718
W. NR.: 2.4668
ASTM: B 637, B 670
ASME: CASE 2222-1, SFA 5.14
AMS: 5596, 5662, 5663, 5832
GE: B50TF14, B50TF15
- Alloy 718
- Inconel® 718
- Nickel 718
- Gas turbine engine parts
- Firearms production
- Liquid fuel rocket motor components
- Springs, fasteners
- Cryogenic tanks
Share This Page