NICKEL
Quote, Buy, Track!
We make it easy to get instant pricing and purchase your metal at the click of a button. Track your order progress, get notified when it ships, and follow your shipment online until it’s delivered. It’s that easy!
Latest Articles
Best Practices When Using Specialty Materials for SWRO Feed and Brine Reject Lines
In our webinar we 8217 ll explore the fascinating journey of stainless steels in SWRO Seawater Reverse Osmosis applications <
2024 Trade Shows
Come talk to a Rolled Alloys representative in person about your project You can find us at these trade shows
Los Angeles Operations Tour
Welcome to Rolled Alloys Los Angeles where our General Manager Carol Plana with nearly two decades of experience leads an
Dual Certification
The term 8220 dual certification 8221 is primarily employed when certifying a material as meeting the specifications for two separate
AL-6XN® / UNS N08367
AL-6XN® / UNS N08367 is a low carbon, high purity, nitrogen-bearing super-austenitic stainless alloy. It was designed to be a seawater resistant material and has since been demonstrated to be resistant to a broad range of corrosive environments.
The high strength and corrosion resistance make it a better choice than the conventional duplex stainless steels and a cost effective alternative to more expensive nickel-base alloys where excellent formability, weldability, strength and corrosion resistance are essential.
The levels of chromium, molybdenum and nitrogen in AL-6XN all serve to provide resistance to acidic oxidizing chloride solutions previously achieved only by the nickel base alloys, and high nickel (24%) and molybdenum (6.3%) contents make AL-6XN an excellent solution to chloride ion stress corrosion cracking. Because of its nitrogen content AL-6XN features greater tensile strength than common austenitic stainless, while retaining high ductility and impact strength. ASME allowable stresses are up to 75% higher than for 316L stainless, and more than twice those for the copper-nickel alloys.
- 6.3% molybdenum
- Over 25 years of proven seawater service
- Practical immunity to chloride stress cracking
- 50% stronger than stainless
- ASME coverage up to 800°F
- Easily welded
- Available in ALL product forms
AL-6XN® is a registered trademark of ATI Properties, LLC, a subsidiary of ATI Inc.
- Excellent resistance to pitting and crevice corrosion in chloride solutions
- Practical immunity to stress corrosion cracking in NaCl environments
- High strength and toughness
UNS: N08367
ASTM: B 688, A 240, B 675, A 312, B 676, A 249, B 804, B 691, A 479, B 462, A 182, B 564, B 366, B 472
ASME: SB 688, SA 240, SB 675, SA 312, SB 276, SA 249, SB 691, SA 479, SB 462, SA 182, SB 564, SB 366 CASE CODE N-438-3, B31.1 CASE 155-1
- FGD Scrubbers
- Reverse Osmosis
- Distillation Columns
- Offshore Oil and Gas
- Heat Exchangers
Share This Page