STAINLESS STEEL
Quote, Buy, Track!
We make it easy to get instant pricing and purchase your metal at the click of a button. Track your order progress, get notified when it ships, and follow your shipment online until it’s delivered. It’s that easy!
Latest Articles
Best Practices When Using Specialty Materials for SWRO Feed and Brine Reject Lines
In our webinar we 8217 ll explore the fascinating journey of stainless steels in SWRO Seawater Reverse Osmosis applications <
2024 Trade Shows
Come talk to a Rolled Alloys representative in person about your project You can find us at these trade shows
Los Angeles Operations Tour
Welcome to Rolled Alloys Los Angeles where our General Manager Carol Plana with nearly two decades of experience leads an
Dual Certification
The term 8220 dual certification 8221 is primarily employed when certifying a material as meeting the specifications for two separate
N-50 (XM-19)
N-50 (XM-19) is a high strength and good corrosion resistant austenitic stainless steel. It has nearly double the yield strength of 304 and 316 stainless steel and has better corrosion resistance than 317L stainless steel. N-50 Stainless remains non-magnetic even after being severely cold worked. It maintains strength at high temperatures as well as sub-zero temperatures.
- High strength austenitic alloy
- Good corrosion resistance
UNS: S20910
W. NR.: 1.3964
ASTM: A 193, A 262, A 276, A 479
AMS: 5764
NACE:MR0175
ISO: 15156
Nitronic 50
- Seawater pump shafts
- Heat exchangers
- Pressure vessels
- Marine hardware