STAINLESS STEEL
Quote, Buy, Track!
We make it easy to get instant pricing and purchase your metal at the click of a button. Track your order progress, get notified when it ships, and follow your shipment online until it’s delivered. It’s that easy!
Latest Articles
Best Practices When Using Specialty Materials for SWRO Feed and Brine Reject Lines
In our webinar we 8217 ll explore the fascinating journey of stainless steels in SWRO Seawater Reverse Osmosis applications <
2024 Trade Shows
Come talk to a Rolled Alloys representative in person about your project You can find us at these trade shows
Los Angeles Operations Tour
Welcome to Rolled Alloys Los Angeles where our General Manager Carol Plana with nearly two decades of experience leads an
Dual Certification
The term 8220 dual certification 8221 is primarily employed when certifying a material as meeting the specifications for two separate
15-5 PH
The 15-5 PH alloy was designed to have greater toughness than 17-4 PH. The 15-5 PH alloy is martensitic in structure in the annealed condition and is further strengthened by a relatively low temperature heat treatment which precipitates a copper containing phase in the alloy. 15-5 PH is also referred to as XM-12 in some specifications.
- Precipitation Hardening
- High Strength
- Moderate corrosion resistance to 600°F
UNS: S15500
W. NR.: 1.4545
ASTM: A 564, A 693, A 698, A 705, A 564, BAC 5439 REV H CLASS A TYPE 1, BMS 7-240 (BOEING), BSS7055 REV A, STD 2154
ASME: SA 564, SA 693, SA 705
AMS: 5659, 5862J TYPE 2
- Aerospace applications
- Chemical and petrochemical applications
- Pulp and paper
- Food processing