NICKEL
Quote, Buy, Track!
We make it easy to get instant pricing and purchase your metal at the click of a button. Track your order progress, get notified when it ships, and follow your shipment online until it’s delivered. It’s that easy!
Latest Articles
Best Practices When Using Specialty Materials for SWRO Feed and Brine Reject Lines
In our webinar we 8217 ll explore the fascinating journey of stainless steels in SWRO Seawater Reverse Osmosis applications <
2024 Trade Shows
Come talk to a Rolled Alloys representative in person about your project You can find us at these trade shows
Los Angeles Operations Tour
Welcome to Rolled Alloys Los Angeles where our General Manager Carol Plana with nearly two decades of experience leads an
Dual Certification
The term 8220 dual certification 8221 is primarily employed when certifying a material as meeting the specifications for two separate
Invar 36
Invar 36 is a nickel-iron, low-expansion alloy containing 36% nickel. It maintains nearly constant dimensions over the range of normal atmospheric temperatures, and has a low coefficient of expansion from cryogenic temperatures to about 500°F. The alloy also retains good strength and toughness at cryogenic temperatures. Invar 36 can be hot and cold formed and machined using processes similar to austenitic stainless steels.
- Low expansion rate up to 500°F
- Readily weldable
UNS: K93600
W. NR.: 1.3912
ASTM: F 1684-06
- Tooling and dies for composite forming
- Cryogenic components
- Laser components