NICKEL
Quote, Buy, Track!
We make it easy to get instant pricing and purchase your metal at the click of a button. Track your order progress, get notified when it ships, and follow your shipment online until it’s delivered. It’s that easy!
Latest Articles
Best Practices When Using Specialty Materials for SWRO Feed and Brine Reject Lines
In our webinar we 8217 ll explore the fascinating journey of stainless steels in SWRO Seawater Reverse Osmosis applications <
2024 Trade Shows
Come talk to a Rolled Alloys representative in person about your project You can find us at these trade shows
Los Angeles Operations Tour
Welcome to Rolled Alloys Los Angeles where our General Manager Carol Plana with nearly two decades of experience leads an
Dual Certification
The term 8220 dual certification 8221 is primarily employed when certifying a material as meeting the specifications for two separate
718 (AMS 5663)
Alloy 718 (AMS 5663) is bar that is already aged (precipitation hardened). As supplied, this material provides higher tensile strength and hardness compared to 718 in the annealed condition. Machining aged 718 is generally more difficult than machining annealed material. The benefit is that once machining is completed the part is complete. Avoiding post machining heat treatment has several benefits since it eliminates the issue of dimensional change during aging. It also provides significant logistical advantages.
- Aged to final heat treat condition
- Good mechanical properties: tensile, fatigue and creep-rupture
- Weldable
- Oxidation resistant throughout its useful temperature range
UNS: N07718
W. NR.: 2.4668
ASTM: B 637
ASME: SB 637
AMS: 5663
GE: B50TF15
- Alloy 718
- Inconel® 718
- Nickel 718
- Gas turbine engine parts
- Liquid fuel rocket motor components
- Firearms production
- Springs, fasteners