STAINLESS STEEL
Quote, Buy, Track!
We make it easy to get instant pricing and purchase your metal at the click of a button. Track your order progress, get notified when it ships, and follow your shipment online until it’s delivered. It’s that easy!
Latest Articles
Best Practices When Using Specialty Materials for SWRO Feed and Brine Reject Lines
In our webinar we 8217 ll explore the fascinating journey of stainless steels in SWRO Seawater Reverse Osmosis applications <
2024 Trade Shows
Come talk to a Rolled Alloys representative in person about your project You can find us at these trade shows
Los Angeles Operations Tour
Welcome to Rolled Alloys Los Angeles where our General Manager Carol Plana with nearly two decades of experience leads an
Dual Certification
The term 8220 dual certification 8221 is primarily employed when certifying a material as meeting the specifications for two separate
RA 253 MA®
The High Strength Heat Resistant Stainless Steel
RA 253 MA® was developed when the need for a heat resistant stainless steel with high strength, while maintaining good oxidation resistance was present in the industry. The lean 11% nickel content of RA 253 MA is a key contributor to being cost effective and stable. With the addition of rare earth elements, RA 253 MA still performs well at temperatures up to 2000°F (1093°C), similar to that of 310 stainless steel.
Performance Profile
RA 253 MA is a lean austenitic heat resistant alloy with high strength and outstanding oxidation resistance. It offers an excellent combination of creep strength along with excellent resistance to oxidation, sulfidation, and erosion at high temperatures in an alloy containing just 11% nickel. Because of its lean chemistry, RA 253 MA is very economical compared to most heat resistant alloys.
RA 253 MA obtains its heat resistant properties by tight control of micro alloy additions. The use of cerium in combination with silicon results in superior oxidation resistance to 2000°F (1093°C). Nitrogen, carbon, and cerium combine to provide creep rupture strength that is double that of type 310 and 309 stainless at 1600°F (871°C).
- Oxidation resistance to 2000°F (1093°C)
- Good resistance to sulfidation
- Superior strength at elevated temperatures
- Good resistance to high temperature abrasion
UNS: S30815
W. NR.: 1.4835
ASTM: A 240, A 276, A 312, A 479
ASME: SA 182, SA 312