The History and Uses of AL-6XN®

In response to the need for a cost-effective alloy that could resist brackish water or seawater environments, stainless alloys with even higher levels of chromium and molybdenum were developed. This need resulted in the development and introduction of AL-6X™ in the early 1970s by ATI.

One significant problem with AL-6X was that the product forms and sizes were limited due to metallurgical reasons. The alloy’s high chromium and molybdenum content rendered AL-6X susceptible to forming sigma phases upon slow cooling between 1000°F – 2100°F. Flat products thicker than 0.1875″ could not be cooled quickly enough to prevent this formation, which would hamper the material’s corrosion resistance and toughness.

Nitrogen was found to be effective in retarding the formation of sigma phase and enhanced the effects of chromium and molybdenum by improving resistance to pitting, crevice corrosion, and stress-corrosion cracking. The figure below shows the times and temperatures that AL-6X and AL-6XN® tend to form sigma phase. Therefore, AL-6XN® was developed as an improvement over AL-6X. Both alloys have the same elemental composition except AL-6XN® contained an intentional addition of 0.18% – 0.25% N.

Sigma Phase Time Temperature Transformation Curves

In 1977, Avesta, now Outokumpu, developed their own super austenitic alloy, 254SMO®, but AL-6XN® became the more widely used and accepted alloy due to a market development relationship with Rolled Alloys. Rolled Alloys played an instrumental role in developing the sources to ensure the supply of all product forms and maintain an inventory of these products in various sizes.

AL-6XN® has various use cases across different industries. It is known for its exceptional performance in coal-fired flue gas desulfurization (FGD) systems and seawater applications in the power industry. Other sectors have also benefited from AL-6XN®’s chloride and acid resistance, leading to increased usage in the chemical process industry (CPI). Additionally, it has shown good resistance to microbiologically influenced corrosion (MIC). The food and pharmaceutical industries have used AL-6XN® for decades in situations where 316/316L was not sufficient. AL-6XN® is also utilized in offshore oil and gas environments, pulp bleaching applications, service water piping, LNG transportation and storage, as well as reverse osmosis desalination systems.

ATI is the only manufacturer with a long-standing history of superior performance, quality, and expertise in producing AL-6XN® (N08637). While other producers have attempted to supply substitute materials that meet the UNS number’s broad chemistry range, they sometimes offer different levels of performance or integrity. Rolled Alloys exclusively stocks genuine AL-6XN® products produced to the highest quality standards.

5-axis waterjet bevel cutting examples, including tapered and angled edges, precision holes, and clean cuts on metal parts.

5-Axis Waterjet Beveling

A 5-axis waterjet cutting machine is an advanced CNC cutting tool that uses a high-pressure stream of water mixed with abrasive (usually garnet) to cut

READ MORE

2026 Trade Show Schedule

Connect with our team in person throughout 2026 at these key industry events. Explore our full trade show schedule to discover where we’ll be exhibiting

READ MORE
Never Miss an Update - Subscribe Today!
Get application insights, material guides, and technical answers straight from the leaders in high-performance alloys.​

Share:

QUOTE, BUY, TRACK

We make it easy to get instant pricing and purchase your metal at the click of a button. Track your order progress, get notified when it ships, and follow your shipment online until it’s delivered. It’s that easy!

Latest Articles

5-Axis Waterjet Beveling

A 5-axis waterjet cutting machine is an advanced CNC cutting tool that uses a high-pressure stream of water mixed with abrasive (usually garnet) to cut through metals and other materials.

Read More »
2026 Trade Show Schedule

Connect with our team in person throughout 2026 at these key industry events. Explore our full trade show schedule to discover where we’ll be exhibiting all year long.

Read More »
How Titanium Sponge and Scrap Become Final Products

Titanium sponge and scrap are the starting materials for producing titanium ingots and slabs. Through processes like vacuum arc remelting (VAR) and hearth melting, these materials are refined into high-purity forms that are then forged, rolled, and finished into titanium plates, bars, and components.

Read More »
Alloying Elements Explained

Alloying elements play a critical role in shaping the strength, corrosion resistance, and performance of metals. This article breaks down the most common alloying elements, explains how they affect material properties, and provides guidance for choosing the right alloy for any application.

Read More »
Privacy Overview

This website uses cookies so that we can provide you with the best user experience possible. Cookie information is stored in your browser and performs functions such as recognising you when you return to our website and helping our team to understand which sections of the website you find most interesting and useful.