Home » News & Articles » Positive Material Identification (PMI)
Positive material identification (PMI) has become more prevalent and practical in recent years. The development of portable X-ray fluorescence (XRF) units using X-ray tubes instead of isotopes has made it easier to verify alloys at the time of final packaging and shipment, at receiving, and in the field.
Portable optical emission spectroscopy (OES) instruments have also become affordable, which permits analysis of even lower molecular weight alloying elements like carbon. However, the most accurate analyses of carbon, nitrogen, and sulfur are still obtained by combustion techniques.
Testing protocols range from performing a spot check on a heat lot of material to obtaining a complete chemistry for every piece. While many of these instruments have exceptional accuracy for portable hand-held units, they cannot match the accuracy of more sophisticated stationary units found in most test laboratories or steelmaking facilities. These limitations should be considered when establishing acceptance criteria. For product analyses, a chemical analysis check to verify the chemistry of a final product using a stationary unit, the permissible variations can be found in ASTM and AMS specifications.
In ASTM, this information can be found in standards such as A480 (stainless steel flat products) or A484 (stainless steel bar). AMS specifications 2248 (steels and stainless steels) and 2269 (nickel and cobalt alloys) detail similar allowances. Product analysis allowances are necessary due to the variability during processing and deviations associated with analytical reproducibility. Additionally, product analysis occurs at a different stage compared to a heat analysis, so this can introduce variability as well. Table 1 shows permitted variations for a few critical elements per ASTM A480. It is best to consult the equipment manufacturer for the associated variation pertaining to portable units.
Table 1: Allowable Variations for a few Critical Elements per ASTM A480
Most modern XRF units also calculate a standard deviation, which displays how precise the measurement might be. By taking the standard deviation and tripling it, then subtracting and adding this value from the measurement displayed on the XRF unit, you can determine a 99.7% range that subsequent tests should fall within for a given element. This method gives a reliable way to predict the expected spread of readings. This vast amount of potential variation in the reading often means that an acceptable chemistry might appear outside the permissible range. For this reason alone, portable instruments should be used only to confirm the alloy type and should not be used as a basis for rejection.
There are many other reasons for the variation of results in chemistries when testing in the field. Part geometry and surface condition can be factors. There are many other reasons for the variation of results in chemistries when testing in the field. Part geometry and surface condition can be factors.
Portable instruments do not penetrate below this surface layer, which might be marginally reduced in chromium, molybdenum, or other elements. Removing several thousandths from the surface to expose base material may be necessary to get a more reliable indication. This effect can also be avoided by taking the reading on a freshly cut edge or end. The reported results also need to be adjusted for interference from other elements. As the alloy content changes, the interference on the reading from other elements also changes. The portable instruments have sophisticated algorithms that compensate for much of this interference. This design allows the portable instruments to work on an extensive range of alloys and compositions.
To improve accuracy, stationary laboratory instruments can be recalibrated using standards specific to the composition being examined. Laboratories in producing mills are the most familiar with compensating for these variations with their alloys, which is why even independent laboratories occasionally have difficulty matching the mill’s accuracy.
Rolled Alloys has portable XRF units in each of our facilities, and we perform hundreds of tests every day. These instruments help verify the alloy’s identity. Material acceptance or rejection based on chemical analysis should only be done using certified laboratories with the most sophisticated equipment and techniques for the elements in question. In case of a dispute or disagreement, the producing mill should always be involved. Please contact Rolled Alloys Quality Assurance if you have questions about our PMI procedures or capabilities.

5-Axis Waterjet Beveling
A 5-axis waterjet cutting machine is an advanced CNC cutting tool that uses a high-pressure stream of water mixed with abrasive (usually garnet) to cut

A Smarter Way to Order Metal Online
Introducing updates to the Rolled Alloys eCommerce experience designed for speed, clarity, and control.

2026 Trade Show Schedule
Connect with our team in person throughout 2026 at these key industry events. Explore our full trade show schedule to discover where we’ll be exhibiting
Never Miss an Update - Subscribe Today!
Get application insights, material guides, and technical answers straight from the leaders in high-performance alloys.
Most modern XRF units also calculate a standard deviation, which displays how precise the measurement might be. By taking the standard deviation and tripling it, then subtracting and adding this value from the measurement displayed on the XRF unit, you can determine a 99.7% range that subsequent tests should fall within for a given element. This method gives a reliable way to predict the expected spread of readings. This vast amount of potential variation in the reading often means that an acceptable chemistry might appear outside the permissible range. For this reason alone, portable instruments should be used only to confirm the alloy type and should not be used as a basis for rejection.
There are many other reasons for the variation of results in chemistries when testing in the field. Part geometry and surface condition can be factors. There are many other reasons for the variation of results in chemistries when testing in the field. Part geometry and surface condition can be factors.
Share:
QUOTE, BUY, TRACK
We make it easy to get instant pricing and purchase your metal at the click of a button. Track your order progress, get notified when it ships, and follow your shipment online until it’s delivered. It’s that easy!
Latest Articles
5-Axis Waterjet Beveling
A 5-axis waterjet cutting machine is an advanced CNC cutting tool that uses a high-pressure stream of water mixed with abrasive (usually garnet) to cut through metals and other materials.
A Smarter Way to Order Metal Online
Introducing updates to the Rolled Alloys eCommerce experience designed for speed, clarity, and control.
2026 Trade Show Schedule
Connect with our team in person throughout 2026 at these key industry events. Explore our full trade show schedule to discover where we’ll be exhibiting all year long.
How Titanium Sponge and Scrap Become Final Products
Titanium sponge and scrap are the starting materials for producing titanium ingots and slabs. Through processes like vacuum arc remelting (VAR) and hearth melting, these materials are refined into high-purity forms that are then forged, rolled, and finished into titanium plates, bars, and components.
Alloying Elements Explained
Alloying elements play a critical role in shaping the strength, corrosion resistance, and performance of metals. This article breaks down the most common alloying elements, explains how they affect material properties, and provides guidance for choosing the right alloy for any application.