Understanding material test reports (MTR) can be challenging for those who seldom need to interpret them. There is no standard format for reporting the required information on an MTR, which leads to mills generating MTRs with varying formats. In some cases, mills indicate their ability to modify their MTR format is limited because of internal system constraints. Although MTRs vary in appearance based on the producing mill, there are commonalities.
Please contact the Rolled Alloys Metallurgical Services group at 1-800-521-0332 or email usย metallurgical-help@demo.rolledalloys.comย if you have additional questions.

2026 Trade Show Schedule
Connect with our team in person throughout 2026 at these key industry events. Explore our full trade show schedule to discover where weโll be exhibiting

How Titanium Sponge and Scrap Become Final Products
Titanium sponge and scrap are the starting materials for producing titanium ingots and slabs. Through processes like vacuum arc remelting (VAR) and hearth melting, these

Alloying Elements Explained
Alloying elements play a critical role in shaping the strength, corrosion resistance, and performance of metals. This article breaks down the most common alloying elements,
Never Miss an Update - Subscribe Today!
Get application insights, material guides, and technical answers straight from the leaders in high-performance alloys.โ
Share:
QUOTE, BUY, TRACK
We make it easy to get instant pricing and purchase your metal at the click of a button. Track your order progress, get notified when it ships, and follow your shipment online until it’s delivered. It’s that easy!
Latest Articles
2026 Trade Show Schedule
Connect with our team in person throughout 2026 at these key industry events. Explore our full trade show schedule to discover where weโll be exhibiting all year long.
How Titanium Sponge and Scrap Become Final Products
Titanium sponge and scrap are the starting materials for producing titanium ingots and slabs. Through processes like vacuum arc remelting (VAR) and hearth melting, these materials are refined into high-purity forms that are then forged, rolled, and finished into titanium plates, bars, and components.
Alloying Elements Explained
Alloying elements play a critical role in shaping the strength, corrosion resistance, and performance of metals. This article breaks down the most common alloying elements, explains how they affect material properties, and provides guidance for choosing the right alloy for any application.
How the Kroll Process Produces Titanium Sponge
The Kroll process is the primary industrial method for transforming titanium ore into metallic titanium…
RA 253 MA Delivers High-Temp Performance in Industry Feature
Rolled Alloys has been featured in Heat Treat Today with the article, โA Microalloyed Solution for High-Temp Applications.โ
Each MTR should have a section identifying the alloy, heat number, specification(s), product form, size, and condition. Unfortunately, the reported condition does not always translate into a clear understanding of what is being supplied. For example, cold finished and cold worked may sound similar but mean different things.
ย
An MTR will also have a chemistry section reporting the ladle analysis of the heat. A second chemistry may also be reported as a check or product analysis. It is common for melt practices to be found in an MTRs chemistry section. On many MTRs, mills will use different abbreviations for different melt practices. Common abbreviations that may be encountered include:
Occasionally, an MTR may report residual elements that are not required to be analyzed. This is permitted and does not mean there is something present that shouldn’t be.
ย
Another section of the MTR will show mechanical properties. The information reported will vary by alloy and by specification requirements. In most instances, an MTR will indicate yield strength (0.2% YS), ultimate tensile strength (UTS), elongation (E%), hardness, and reduction of area (RA%). Some materials require Charpy impact toughness testing if they are known to undergo a ductile-to-brittle transition at low temperatures.
ย
For thermally hardenable materials, an MTR will contain a capability testing section. Capability testing involves taking samples of the supplied material and heat-treating them, often to a specific specification’s requirements, to demonstrate the materials’ ability to achieve the required properties. For martensitic grades (410, 416, 420, 440C), the capability section often contains a hardness reading. For precipitation hardenable grades (17-4, 15-5, 13-8), aged room temperature tensile properties will be listed. Some thermally hardenable materials like 718 will require elevated temperature capability testing. This can involve elevated tensile tests as well as stress rupture testing. At elevated temperatures, loads below the yield strength can cause materials to elongate and fail over time. These tests may take several days to complete, and the results are usually reported in hours to failure. More than one set of properties may be reported if testing is done to more than one specification. The results will generally be distinguished by the heat treatment parameters used to determine the capability. Remember that capability test results are from heat-treated samples and do not represent the supplied condition.
Depending on the specification purchased to or purchase order requirements, MTRs may report grain size, results of corrosion testing, magnetic properties, and more. With so many different styles, languages, and terms, even veteran metallurgists may need extra time to decipher the results of an MTR. If you need help understanding an MTR, don’t hesitate to contact Rolled Alloys Metallurgical Services or QA.