Home » News & Articles » Introduction to Heat Resistant Alloys
We have been supporting the heat-resistant alloy market for over 70 years. Many different industries, such as thermal processing, chemical processing, and power generation, depend on the capabilities of these alloys to perform day-to-day activities.
In this webinar, we will explore the world of wrought heat-resistant alloys. The listener will be introduced to commonly utilized heat-resistant alloys, factors to consider when selecting a heat-resistant alloy, and some industrial applications within specific industries.
Presentation Slides
Exploring the World of High-Temperature Alloys
Welcome to Rolled Alloys’ Webinar Series
Hello and welcome to Rolled Alloys’ second webinar in our ongoing series. In today’s session, we’re delving into the fascinating world of heat-resistant alloys. Whether you’re a materials enthusiast or someone seeking specific solutions for high-temperature applications, we’ve got you covered.
In this blog post, we will cover key takeaways from the webinar, explore the fundamental aspects of heat-resistant alloys, and discuss their applications. We will also touch upon some important considerations when choosing the right materials for your specific needs.
Rolled Alloys: Your Trusted Global Supplier
Before we dive into the world of heat-resistant alloys, it’s essential to know who we are. Rolled Alloys is a global supplier specializing in high-performance alloys. Our offering includes state-of-the-art material processing, an exceptional e-commerce platform, and a team of metallurgical experts to assist you. We provide a wide range of alloys, including nickel alloys, stainless steels, duplex, titanium, cobalt, and various forms such as plates, sheets, and bars.
What Are Heat-Resistant Alloys?
Heat-resistant alloys are a special group of materials designed for high-temperature environments. These alloys contain a minimum of 12% chromium to form a protective chromium oxide layer at high temperatures. Additional elements such as carbon, nitrogen, nickel, silicon, and aluminum enhance their properties. Rare earth metals are also incorporated to improve oxide adherence.
Some common heat-resistant alloys include,
Factors to Consider When Selecting Heat-Resistant Alloys
- Oxidation Resistance: Heat-resistant alloys with at least 12% chromium can form an oxide layer that protects them at high temperatures. Beyond the oxidation threshold, they become porous and brittle.
- Creep Strength: Creep is time-dependent deformation at elevated temperatures and constant stress. High creep strength alloys retain their shape, making them ideal for high-temperature applications.
- Carburizing and Nitriding: These processes introduce carbon and nitrogen into the material’s surface, enhancing wear resistance. Alloys with high nickel content are better suited for these environments.
- Vacuum Processing: The process environment should be void of oxygen. Therefore, high temperature oxidation does not tend to be a concern.
Common Applications of Heat-Resistant Alloys
- Thermal Processing: Used for bar baskets, serpentine grids, radiant tubes, and retorts.
- Chemical Processing: Used for flair tips, piping, steam methane reformers, and heat exchangers.
- Galvanizing Lines: Used for their corrosion resistance.
Heat-resistant alloys are also used in a wide range of industries including:
- Power Generation
- Aerospace
- Oil and Gas
- Steel Manufacturing
Conclusion
Heat-resistant alloys are at the heart of numerous high-temperature applications. Understanding their properties and how they behave in various environments is crucial to making the right material selection.
We hope this blog post has provided you with valuable insights into the world of heat-resistant alloys. If you have any questions or need further assistance, please don’t hesitate to reach out to us. You can contact us via email or phone, and we’ll be happy to help. 1-800-521-0332 or email us: metallurgical-help@demo.rolledalloys.com

5-Axis Waterjet Beveling
A 5-axis waterjet cutting machine is an advanced CNC cutting tool that uses a high-pressure stream of water mixed with abrasive (usually garnet) to cut

A Smarter Way to Order Metal Online
Introducing updates to the Rolled Alloys eCommerce experience designed for speed, clarity, and control.

2026 Trade Show Schedule
Connect with our team in person throughout 2026 at these key industry events. Explore our full trade show schedule to discover where we’ll be exhibiting
Never Miss an Update - Subscribe Today!
Get application insights, material guides, and technical answers straight from the leaders in high-performance alloys.
Share:
QUOTE, BUY, TRACK
We make it easy to get instant pricing and purchase your metal at the click of a button. Track your order progress, get notified when it ships, and follow your shipment online until it’s delivered. It’s that easy!
Latest Articles
5-Axis Waterjet Beveling
A 5-axis waterjet cutting machine is an advanced CNC cutting tool that uses a high-pressure stream of water mixed with abrasive (usually garnet) to cut through metals and other materials.
A Smarter Way to Order Metal Online
Introducing updates to the Rolled Alloys eCommerce experience designed for speed, clarity, and control.
2026 Trade Show Schedule
Connect with our team in person throughout 2026 at these key industry events. Explore our full trade show schedule to discover where we’ll be exhibiting all year long.
How Titanium Sponge and Scrap Become Final Products
Titanium sponge and scrap are the starting materials for producing titanium ingots and slabs. Through processes like vacuum arc remelting (VAR) and hearth melting, these materials are refined into high-purity forms that are then forged, rolled, and finished into titanium plates, bars, and components.
Alloying Elements Explained
Alloying elements play a critical role in shaping the strength, corrosion resistance, and performance of metals. This article breaks down the most common alloying elements, explains how they affect material properties, and provides guidance for choosing the right alloy for any application.