Hydrogen Sulfide -MR0175/ISO 15156 & MR0103

NACE International has developed two significant standards relative to the use of materials in hydrogen sulfide-bearing environments.

MR0175/ISO 15156, Petroleum and Natural Gas Industries – Materials for use in H2S-containing Environments in Oil and Gas Production; and MR0103, Materials Resistant to Sulfide Stress Cracking in Corrosive Petroleum Refining Environments. Hydrogen sulfide is a poisonous gas and can cause stress corrosion cracking in steels and alloys. These standards define material limits suitable for use in hydrogen sulfide service conditions.

Stainless steels and select nickel alloys supplied by Rolled Alloys are suitable for use in hydrogen sulfide environments and may be ordered to satisfy these requirements.

300 series austenitic stainless steels are specified to โ€œcontain the following elements in the following proportions, expressed as mass fractions: C, 0.08 % max; Cr, 16 % min; Ni, 8 % min; P, 0.045 % max; S, 0.04 % max; Mn, 2.0 % max; and Si, 2.0 % max. Other alloying elements are permitted.โ€ As a group, the following restrictions, as presented in Table A.2, apply:

– The material must be solution annealed and quenched or annealed and thermally stabilized.

– The material must be free of cold work intended to enhance mechanical properties.

– A maximum hardness of 22 HRC (237 HBW) applies.

These requirements are identical to those for MR0103. All 300 series austenitic stainless steels supplied by Rolled Alloys for stock are produced to standard ASTM/ASME specifications, primarily A/SA 240 for flat products and A/SA 479 for long products. These standards require the material to be supplied in the annealed and quenched condition. Rolled Alloys does not enhance the mechanical properties of these products through cold work. Provided the hardness values reported on the material test report reflect hardness levels below 22 HRC (237 HBW), these materials comply with MR0175 Table A.2 and MR0103 Section 13.5.

AL-6XNยฉ (UNS N08367) is a material of Type 3b. AL-6XN is supplied in the solution annealed condition and satisfies the requirements of Table A.8. Therefore, MR0175 does not require a hardness to be reported for annealed AL-6XN. AL-6XN also meets the requirements of MR0103 Section 13.7 provided the reported hardness is at or below 35 HRC.

Alloy 625 (N06625) provided by Rolled Alloys is annealed and satisfies the requirements outlined in Table A.13 of MR0175. Therefore, MR0175 does not require a hardness to be reported for annealed material. In addition, 625 and 600 conform to MR0103 Section 14.1.1, provided the reported hardness is at or below 35 HRC.

Duplex alloys 2205 (S31803/S32205) and ZERONยฎ 100 (S32760) supplied by Rolled Alloys are provided in the annealed and quenched condition and have a ferrite content between 35% and 65%. As such, they satisfy the requirements for these materials, as stated in Table A.24 of MR0175. Therefore, MR0175 does not require a hardness to be reported for annealed material. These materials also satisfy MR0103, Section 13.8.1, provided the reported hardness is at or below 28 HRC.

All the tables specify any and all limitations for use. These limits include temperatures, partial pressures of H2S, chloride concentrations, pH, comments, and any additional restrictions or requirements.

Since all these materials are supplied to specifications that ensure compliance with the MR0175 requirements, the producing mills may not show MR0175 compliance on test reports. One can verify compliance by asking one of the Rolled Alloys Metallurgical Services staff.

Never Miss an Update - Subscribe Today!

Get application insights, material guides, and technical answers straight from the leaders in high-performance alloys.โ€‹

Share:

QUOTE, BUY, TRACK

We make it easy to get instant pricing and purchase your metal at the click of a button. Track your order progress, get notified when it ships, and follow your shipment online until it’s delivered. It’s that easy!

Latest Articles

We're Here to Help!

Rolled Alloysโ€™ Metallurgical Services team is here to provide answers to your technical questions. This form is not for quoting or purchasing. If you need a quote, log in here.

Privacy Overview

This website uses cookies so that we can provide you with the best user experience possible. Cookie information is stored in your browser and performs functions such as recognising you when you return to our website and helping our team to understand which sections of the website you find most interesting and useful.