Home » News & Articles » Understanding P-Numbers and F-Numbers in Welding
What Are P and F Numbers?
P and F numbers are common within the welding industry, particularly for projects that strictly adhere to codes and standards set in place by ASME.
As this is the case, there is often confusion about P and F numbers regarding what they are, how they are assigned, and why they are important, which this blog aims to answer.
P-numbers are classifications assigned to base metals, which these numbers are used to group base metals with similar welding characteristics. By grouping materials with similar welding characteristics, it helps reduce the number of welding procedure qualifications required. P-numbers are part of ASME Boiler and Pressure Vessel Code (BPVC) Section IX and can be found in Table QW-422.
P-numbers are organized into ranges, which correspond to different alloy classes. Below are the respective ranges for each of the classes:
- P-1 to P-15F: Ferrous alloys
- P-21 to P-26: Aluminum alloys
- P-31 to P-35: Copper alloys
- P-41 to P-49: Nickel alloys
- P-51 to P-53: Titanium alloys
- P-61 to P-62: Zirconium alloys
Within P-numbers are subsets called group numbers, which are assigned to ferrous-based metals requiring toughness testing. These group numbers further classify materials based on their specific properties and requirements for welding.
F-numbers are classifications assigned to filler metals (such as electrodes and bare wire) to reduce the number of WPS and welder performance criteria. F-numbers help group filler metals based on their operational characteristics, which affects a welder’s ability to use them effectively. Like P-numbers, F-numbers can be found in ASME BPVC Section IX but in Table QW-432.
F-number classification reflects factors such as ease of use, welding position, and the skill level required to operate the filler metal effectively. So, higher F-numbers typically indicate a need for more advanced welding skills. Below are the respective ranges for each of the classes:
- F1 to F5: SMAW electrodes
- F6: Any ferrous solid or cored wire
- F21 to F25: Aluminum and aluminum alloys
- F31 to F37: Copper and copper alloys
- F41 to F46: Nickel and nickel alloys
- F51 to F56: Titanium and titanium alloys
- F61: Zirconium and zirconium alloys
- F71 to F72: Hard-facing alloys
The P-numbers for the base materials that Rolled Alloys stocks and the associated F numbers for the fillers used to weld these base materials can be found on our Welding Information page.
Why are P and F Numbers Important?
P and F numbers are important for a variety of reasons. Some of these reasons include:
- Streamline material selection: Engineers and welding specialists can more easily select appropriate materials and welding consumables based on these standardized groupings.
- Standardize welder qualifications: Welder qualifications are often based on P-numbers and F-numbers, allowing welders qualified on one material to work on others within the same group.
- Facilitate code compliance: Many welding codes and standards, like ASME Boiler and Pressure Vessel Code, use P-numbers and F-numbers in their requirements.
- Improve safety and quality: These systems help maintain weld quality and structural integrity by ensuring proper material and filler metal combinations.
Do All Base Materials and Fillers Have a P or F Number?
Not all alloys and filler metals have a P-number or F-number. P-numbers are assigned to base metals to categorize them based on similar weldability and mechanical properties, while F-numbers are assigned to filler metals based on their usability characteristics. However, some materials, particularly those not commonly used in pressure vessels or piping, may not have assigned P-numbers or F-numbers. For instance, certain specialized alloys or materials used in niche applications might not be listed in the ASME BPVC tables.

5-Axis Waterjet Beveling
A 5-axis waterjet cutting machine is an advanced CNC cutting tool that uses a high-pressure stream of water mixed with abrasive (usually garnet) to cut

A Smarter Way to Order Metal Online
Introducing updates to the Rolled Alloys eCommerce experience designed for speed, clarity, and control.

2026 Trade Show Schedule
Connect with our team in person throughout 2026 at these key industry events. Explore our full trade show schedule to discover where we’ll be exhibiting
Never Miss an Update - Subscribe Today!
Get application insights, material guides, and technical answers straight from the leaders in high-performance alloys.
Share:
QUOTE, BUY, TRACK
We make it easy to get instant pricing and purchase your metal at the click of a button. Track your order progress, get notified when it ships, and follow your shipment online until it’s delivered. It’s that easy!
Latest Articles
5-Axis Waterjet Beveling
A 5-axis waterjet cutting machine is an advanced CNC cutting tool that uses a high-pressure stream of water mixed with abrasive (usually garnet) to cut through metals and other materials.
A Smarter Way to Order Metal Online
Introducing updates to the Rolled Alloys eCommerce experience designed for speed, clarity, and control.
2026 Trade Show Schedule
Connect with our team in person throughout 2026 at these key industry events. Explore our full trade show schedule to discover where we’ll be exhibiting all year long.
How Titanium Sponge and Scrap Become Final Products
Titanium sponge and scrap are the starting materials for producing titanium ingots and slabs. Through processes like vacuum arc remelting (VAR) and hearth melting, these materials are refined into high-purity forms that are then forged, rolled, and finished into titanium plates, bars, and components.
Alloying Elements Explained
Alloying elements play a critical role in shaping the strength, corrosion resistance, and performance of metals. This article breaks down the most common alloying elements, explains how they affect material properties, and provides guidance for choosing the right alloy for any application.