Home ยป News & Articles ยป 70 years in the Thermal Processing Industry
Over the past 70 years, Rolled Alloys has been committed to servicing the thermal processing industry.
In 1953, the year the company was founded, we introduced RA330ยฎ as a wrought replacement to cast HT. Due to RA330ยฎ’s versatility and availability, it remains the most widely used wrought alloy by commercial heat treaters.
Key features of RA330ยฎ include:
- Oxidation resistance up to 2100ยฐF
- Creep strength up to 1800ยฐF
- Sufficient nickel to prevent sigma phase formation
- Good thermal shock resistance
Applications where RA330ยฎ commonly finds use include:
- Heat treatment fixtures
- Muffles
- Retorts
- Shaker Hearths
- Radiant Tubes
Although RA330 exhibits excellent features, there may be better choices for an application. With this being the case, we offer a wide range of heat-resistant alloys to best suit the needs of your application.
RA 602 CAยฎ is an alloy developed specifically for the highest temperature process, requiring strength and resistance to atmospheres. Many heat-resistant alloys are out in the world, but when considering availability and capabilities, RA 602 CAยฎ is often unmatched.
Key features of RA 602 CAยฎ include:
- Oxidation resistance up to 2250ยฐF
- Usable creep strength up to 2100ยฐF
- Great resistance to carburization and nitriding
- Immune to sigma phase formation
- Continuous alumina sub-oxide former
Applications where RA 602 CAยฎ commonly finds use include:
- High-temperature muffles, retorts, and radiant tubes
- Rotary calciners
- Vacuum furnace fixtures
- High carbon potential environments
One last alloy worth discussing is RA253MA. RA253MA is a lean, heat-resistant stainless steel with high strength and oxidation resistance. With excellent high-temperature properties and low nickel content, RA253MA is a cost-effective material that thermal processors frequently utilize for open-air applications.
Key features of RA 253ย MAยฎ include:
- Oxidation resistance up to 2000ยฐF
- Usable creep strength up to 2000ยฐF
Applications where RA 253ย MAยฎ commonly finds use include:
- Muffles
- Annealing fixtures
- Wire belts
- Electrically heated calciners
In addition to the alloys discussed in this blog, Rolled Alloys stocks many other heat-resistant alloys, including 309, 310, 800H/AT, 600, 230, 601, and Alloy X. Information on these alloys can be found on each of their respective alloy pages.

2026 Trade Show Schedule
Connect with our team in person throughout 2026 at these key industry events. Explore our full trade show schedule to discover where weโll be exhibiting

How Titanium Sponge and Scrap Become Final Products
Titanium sponge and scrap are the starting materials for producing titanium ingots and slabs. Through processes like vacuum arc remelting (VAR) and hearth melting, these

Alloying Elements Explained
Alloying elements play a critical role in shaping the strength, corrosion resistance, and performance of metals. This article breaks down the most common alloying elements,
Never Miss an Update - Subscribe Today!
Get application insights, material guides, and technical answers straight from the leaders in high-performance alloys.โ
Share:
QUOTE, BUY, TRACK
We make it easy to get instant pricing and purchase your metal at the click of a button. Track your order progress, get notified when it ships, and follow your shipment online until it’s delivered. It’s that easy!
Latest Articles
2026 Trade Show Schedule
Connect with our team in person throughout 2026 at these key industry events. Explore our full trade show schedule to discover where weโll be exhibiting all year long.
How Titanium Sponge and Scrap Become Final Products
Titanium sponge and scrap are the starting materials for producing titanium ingots and slabs. Through processes like vacuum arc remelting (VAR) and hearth melting, these materials are refined into high-purity forms that are then forged, rolled, and finished into titanium plates, bars, and components.
Alloying Elements Explained
Alloying elements play a critical role in shaping the strength, corrosion resistance, and performance of metals. This article breaks down the most common alloying elements, explains how they affect material properties, and provides guidance for choosing the right alloy for any application.
How the Kroll Process Produces Titanium Sponge
The Kroll process is the primary industrial method for transforming titanium ore into metallic titanium…
RA 253 MA Delivers High-Temp Performance in Industry Feature
Rolled Alloys has been featured in Heat Treat Today with the article, โA Microalloyed Solution for High-Temp Applications.โ